| Код ТН ВЭД | 559211 |
| Density | 0.960 g/cm3 |
| Melt Mass Flow Rate | 0.7 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 26 MPa |
| Tensile Strength At Break | 30 MPa |
| Tensile Elongation At Yield | 10% |
| Tensile Elongation At Break | 500% |
| Flexural Modulus | 1.20 GPa |
| Notched Izod Impact Strength | 80 J/m |
| Shore D Hardness | 65 |
| Vicat Softening Temperature | 125 °C |
| Heat Deflection Temperature | 75 °C |
| Melting Temperature | 130 °C |
| Brittleness Temperature | -70 °C |
| Environmental Stress Crack Resistance | 1000 h |
| Water Absorption | 0.01% |
| Mold Shrinkage | 2.0% |
| Specific Gravity | 0.960 |
| Bulk Density | 0.58 g/cm3 |
| Coefficient Of Linear Thermal Expansion | 0.00012 cm/cm/°C |
| Thermal Conductivity | 0.45 W/m-K |
| Volume Resistivity | 1E16 ohm-cm |
| Dielectric Strength | 20 kV/mm |
| Dielectric Constant | 2.3 |
| Dissipation Factor | 0.0002 |
| Arc Resistance | 120 s |
| Oxygen Index | 17% |
Как аккредитованный завод Bamberger Polymers HDPE 0760, мы соблюдаем строгие протоколы качества - каждая партия подвергается строгим испытаниям для обеспечения последовательных стандартов эффективности и безопасности.
| Упаковка | Bamberger Polymers HDPE 0760 is supplied in 55 lb (25 kg) polyethylene bags, palletized and shrink-wrapped. |
| Погрузка контейнера (20-футовый контейнер) | 20′ FCL container loading for Bamberger Polymers HDPE 0760: palletized 25 kg bags, shrink-wrapped, dry container, evenly distributed, properly secured. |
| Доставка | Bamberger Polymers HDPE 0760 is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg bags or bulk containers. Not regulated for DOT, IMDG, or IATA transport. Keep dry, protected from sunlight, heat, and contamination; handle with standard industrial precautions. Ensure packaging remains intact during transit. |
| Хранение | Store Bamberger Polymers HDPE 0760 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, and ignition sources. Keep original bags or containers sealed, off the floor, and protected from moisture, dust, and contamination. Avoid contact with strong oxidizing agents. Use first-in, first-out stock rotation and handle with appropriate personal protective equipment. |
| Срок годности | Typically two years from date of manufacture when stored in original packaging, cool, dry, and away from direct sunlight and moisture. |
Конкурентоспособные цены Bamberger Polymers HDPE 0760, которые соответствуют вашему бюджету - гибкие условия и индивидуальные котировки для каждого заказа.
Для получения образцов, цен или более подробной информации свяжитесь с нами по адресу +8618005193850 или отправить по почте sales8@ascent-chem.com.
Мы ответим вам как можно скорее.
Телефон: +8618005193850
Электронная почта: sales8@ascent-chem.com
Гибкие условия оплаты, конкурентоспособные цены, первоклассное обслуживание — обращайтесь прямо сейчас!