Продукты

Clariant High Impact Polystyrene Grey 3D Printer Filament

    • Название продукта: Clariant High Impact Polystyrene Grey 3D Printer Filament
    • Сайт Factroy: Округ Юду, Ганьчжоу, Цзянси, Китай
    • Запрос цены: admin@ascent-chem.com
    • Производитель: Ascent Petrochem Holdings Co., Limited
    • Свяжитесь сейчас
    Спецификации
    Код ТН ВЭД 716924

    Как аккредитованный завод Clariant High Impact Polystyrene Grey 3D Printer Filament, мы соблюдаем строгие протоколы качества - каждая партия подвергается строгим испытаниям для обеспечения последовательных стандартов эффективности и безопасности.

    Упаковка и хранение
    Упаковка Sealed foil bag containing one 1 kg spool of grey Clariant high-impact polystyrene 3D printer filament, packed in a cardboard box.
    Погрузка контейнера (20-футовый контейнер) 20′ FCL container loaded with palletized Clariant High Impact Polystyrene Grey 3D Printer Filament, secured for dry, safe, compliant transport.
    Доставка Clariant High Impact Polystyrene Grey 3D Printer Filament is shipped as a non-hazardous, non-regulated article. Spools are sealed with desiccant in moisture-barrier bags, cushioned in sturdy cartons. Standard ground or air service applies. Store dry, away from heat, sunlight, and static. Carrier and rate depend on package dimensions and weight.
    Хранение Store Clariant High Impact Polystyrene Grey 3D Printer Filament in a cool, dry, well-ventilated area, ideally in its original sealed, moisture-barrier packaging with desiccant. Keep away from direct sunlight, heat, sparks, open flames, and incompatible solvents. Maintain low humidity to prevent moisture absorption; reseal partially used spools in airtight containers. Use first-in, first-out stock rotation.
    Срок годности Shelf life is about 12–24 months if unopened, stored cool, dry, sealed, and protected from moisture and UV light.
    Применение Clariant High Impact Polystyrene Grey 3D Printer Filament

    Clariant High Impact Polystyrene Grey 3D Printer Filament is a styrenic feedstock supplied in 1.75 mm or 2.85 mm diameter. Downstream processing in this document is limited to non-food-contact and non-implantable fused deposition modelling routes. Published data for this specific grey Clariant compound are limited. The process windows below draw from generic HIPS extrusion grades verified under ISO and ASTM methods. Batch-specific certificates should be requested from the compounder for the grey masterbatch, stabiliser package, and lot-to-lot melt flow deviation.

    Typical HIPS extrusion-grade property ranges
    PropertyMethodReported range
    DensityISO 1183-1:20191.03–1.05 g/cm³
    Melt flow index, 200 °C, 5 kgISO 1133-1:20223–8 g/10 min
    Tensile yield stressISO 527-2:201220–28 MPa
    Tensile elongation at breakISO 527-2:201230–60 %
    Flexural modulusISO 178:20191800–2300 MPa
    Charpy notched impact, 23 °CISO 179-1:20106–12 kJ/m²
    Vicat softening point, method A50ISO 306:202284–94 °C
    Heat deflection temperature, 1.8 MPaISO 75-2:201375–85 °C

    Clariant HIPS grey filament is used as a snap-away and solvent-removable support material in dual-extrusion builds where ABS, ASA, or HIPS primary bodies are printed. The styrenic backbone reduces interfacial adhesion to a practical breakaway level rather than forming a permanent bond. The support-to-model interface gap is set at 0.2 mm to 0.4 mm. Support density is held at 12 % to 18 % for dissolvable structures. Support densities above 25 % extend solvent removal beyond 8 h and increase limonene uptake into the primary part. Primary ABS is extruded at 235 °C to 245 °C. Support HIPS is extruded at 230 °C to 240 °C. A borosilicate glass or PEI film bed is held at 95 °C to 105 °C. Enclosure air temperature is maintained at 40 °C to 45 °C. The filament is dried at 70 °C for 2 h if ambient relative humidity exceeds 60 %. Residual HIPS is dissolved in d-limonene, CAS 5989-27-5, at 45 °C to 55 °C in a 40 kHz ultrasonic bath. A 2 mm support shell typically requires 2 h to 6 h for full removal, depending on channel diameter and solvent saturation. d-Limonene is not an aggressive solvent for ABS at short exposure, but becomes a stress-cracking agent when ABS is immersed for more than 12 h at 55 °C. High-stress ABS snap-fit features should be limited to under 4 h of contact and rinsed with isopropanol. Compliance is evaluated at the resin level under RoHS 2011/65/EU Annex II and REACH Regulation (EC) No 1907/2006 SVHC declarations. Terminal products are ABS or ASA housings, ducting, and brackets with clean internal channels and no residual support material.

    What Processing Ceiling Applies to Grey HIPS Masters in PETG Vacuum Forming?

    Vacuum forming tools printed from Clariant HIPS grey filament are restricted to low-temperature sheet materials such as PETG processed at 90 °C to 110 °C. HIPS softens at a Vicat point of 84 °C to 94 °C under method ISO 306 A50. A PETG sheet heated to 110 °C transfers heat into the tool surface within 20 s to 40 s. A printed tool with 3 mm skin thickness reaches 65 °C to 75 °C on the contact face if the backside is actively cooled. Without cooling, the contact face exceeds 85 °C after 8 to 12 pulls. Surface flattening and vacuum-hole closure then occur. The tool shell should be at least 4 mm thick. Vent holes are drilled at 0.5 mm diameter with a pitch of 20 mm. The printed surface is sealed with a two-component epoxy coating of 250 μm to 300 μm dry film thickness. This coating fills layer valleys and resists drag from release agents. The printed insert is mounted in an aluminium frame to reduce flexure. Dry sanding above 400 grit requires dust extraction because styrene monomer release is controlled under REACH. Terminal products are PETG trays, low-temperature blister prototypes, and packaging inserts. Published data for this specific Clariant grey HIPS configuration in vacuum forming is limited. The above values reflect generic HIPS extrusion-grade behaviour and require batch-specific validation.

    Burnout behaviour of grey HIPS sacrificial patterns is governed by ash content and thermal expansion mismatch. The pattern is printed at 0.1 mm layer height with 5 % to 10 % infill to reduce shell stress during the thermal ramp. The printed pattern is mounted on a standard wax sprue and coated with a refractory slurry based on colloidal silica and zircon flour. A typical shell build uses 7 to 10 coats. Particle size decreases from 200 μm to 45 μm. After shell drying at 22 °C and 50 % RH for 48 h, the HIPS pattern is removed in a kiln. The kiln schedule is constrained by the thermal expansion of polystyrene, approximately 70 × 10⁻⁶ K⁻¹ to 80 × 10⁻⁶ K⁻¹ by ISO 11359-2. A ramp rate above 2 °C/min between 90 °C and 120 °C can crack the primary coat. A burnout plateau at 250 °C for 1 h allows depolymerisation before the final ramp to 650 °C for 2 h. Ash residue for unfilled PS is reported below 0.5 wt%. Grey masterbatch may raise ash marginally. Published data for this specific pigment package is limited. Slurry binder pH is held at 9.0 to 10.0 to avoid reaction with residual styrene vapour. Terminal products are low-alloy steel and aluminium investment-cast components. This route is not qualified for high-integrity aerospace castings without independent ash and shell permeability validation.

    RTV Silicone Mould Masters and Surface Inhibitor Testing

    Room-temperature-vulcanising silicone rubbers reproduce fine surface detail from Clariant HIPS grey filament masters. The printed master is sanded from 180 grit to 600 grit. It is then primed with a high-solids urethane sealer at 30 % to 40 % volume solids. The sealer prevents low-molecular-weight styrene and grey pigment particles from migrating into platinum-cure silicone. Migration can poison the hydrosilylation catalyst and produce a tacky mould surface. A small-batch cure test on a sealed HIPS coupon is required before full mould pour. The mixing ratio for a standard addition-cure RTV silicone is 10:1 by weight of Part A to Part B. Vacuum degassing is carried out at -0.09 MPa for 5 min. Pour thickness over the pattern is 8 mm to 12 mm. Cure is carried out at 23 °C for 18 h to 24 h. Post-cure at 60 °C for 2 h is applied only if the sealed HIPS master can tolerate 60 °C without deformation. The grey surface improves visual contrast for detecting air bubbles in translucent silicone. Terminal products are polyurethane casting moulds, wax masters, and cold-cast decorative components. REACH applies to monomer content in the sealer. The printed HIPS master is not a food-contact article.

    When Limonene Vapour Smoothing Is Specified for Exhibition Models

    Solvent smoothing of HIPS grey prints is performed in a closed chamber with d-limonene heated to 40 °C. The part is suspended above the liquid rather than immersed. Vapour concentration is controlled by chamber volume and liquid surface area. A ratio of 1 mL d-limonene per 2 L chamber volume at 40 °C is a practical starting point. Exposure time is 15 min to 30 min for a 0.2 mm layer height print. Smoothing reduces surface roughness from Ra 15 μm to Ra 3 μm to 6 μm. Dimensional loss occurs on sharp edges. Features below 0.5 mm width are rounded beyond 0.1 mm. After smoothing, parts are dried at 20 °C to 22 °C for 12 h before painting. A two-pack polyurethane primer is applied at 20 μm dry film thickness. The grey base provides neutral colour for light-coloured topcoats. d-Limonene is a skin and eye irritant. The vapour is heavier than air and can accumulate in low points. Local exhaust ventilation and nitrile gloves are required. Terminal products are architectural models, exhibition models, and paint-ready visual prototypes.

    Non-load-bearing enclosures and prototype chassis printed from Clariant HIPS grey filament are used for board-fit validation before injection moulding. The material is not rated as a continuous electrical insulator. Flammability classification is UL 94 HB at 1.5 mm and 3.0 mm thickness. Solvent-based conformal coatings may attack the styrenic surface. Adhesion testing is required before anti-static or EMI shielding coatings are applied. Thread-forming screws are installed into printed bosses with a pilot hole of 2.6 mm for M3 screws. Boss outer diameter should be 2.5 times the screw diameter to resist splitting. Printing parameters are 0.2 mm layer height, 4 perimeters, and 25 % rectilinear infill. No load-bearing boss should exceed 5 kg at 23 °C. Terminal products are functional enclosures, rack ear prototypes, and cable routing fixtures. Compliance of the printed prototype does not transfer to the final injection-moulded article. The final article must be re-evaluated for UL 94, CE EMC, and applicable electrical enclosure standards.

    Бесплатная цитата

    Конкурентные цены Clariant High Impact Polystyrene Grey 3D Printer Filament, которые соответствуют вашему бюджету - гибкие условия и индивидуальные котировки для каждого заказа.

    Для получения образцов, цен или более подробной информации свяжитесь с нами по адресу +8618136850665 или отправить по почте admin@ascent-chem.com.

    Мы ответим вам как можно скорее.

    Телефон: +8618136850665

    Электронная почта: admin@ascent-chem.com

    Запрос

    Получите бесплатную сметуAscent Petrochem Holdings Co., Limited

    Гибкие условия оплаты, конкурентоспособные цены, первоклассное обслуживание — обращайтесь прямо сейчас!

    Сертификация и соответствие требованиям
    Более подробное введение

    Clariant High Impact Polystyrene Grey 3D Printer Filament is an unfilled impact-modified styrenic feedstock supplied for fused filament fabrication. The product is generally offered in 1.75 mm and 2.85 mm nominal diameters on vacuum-sealed spools, with distributor-reported net spool masses of 750 g or 2.3 kg depending on the regional SKU. The base resin is a graft copolymer of styrene and polybutadiene rubber in a two-phase morphology; the grey tint is produced with a light-stable pigment package rather than mineral filler. The grey masterbatch is added at a let-down ratio below 1.0 wt%; the formulation remains mineral-free, and the ash content measured by ISO 3451-1:2019 method A on the compounded granulate is typically below 0.1 wt%. The material code is distributor-specific, and the lot-specific identifier on the vacuum-sealed label should be used for incoming traceability. Published data for this specific product configuration is limited, so the bounding values cited in this document are representative of unfilled high-impact polystyrene extrusion grades conforming to ISO 2897-1 and should be confirmed against the lot-specific batch certificate. The filament is distinguished from general-purpose HIPS by tighter control of melt volume-flow rate, dimensional ovality, and residual monomer, which are reported on supplier certificates using ISO 1133-1:2022 and laser-micrometer methods. Its primary dual-mode use is as a structural styrenic part or as a solvent-removable support in dual-extruder architectures, particularly where the paired model material is ABS or ASA and where water-soluble PVA support is rejected because of humidity-sensitive re-softening and poor styrenic adhesion.

    The technical positioning of the filament depends on three processing parameters: melt temperature, bed and chamber heat uniformity, and moisture uptake history. HIPS absorbs less water than polyamide or PVA, but prolonged exposure to high relative humidity can still produce visible nozzle sputter and microvoids at layer boundaries. The grey grade is therefore dried at 60 °C for 3–4 h if spools have been stored outside a sealed bag at 60% RH for more than 48 h. The recommended processing window on standard FFF equipment is narrow enough that uncontrolled chamber temperature fluctuations of more than ±5 °C around the setpoint can alter the shrinkage profile across a 200 mm footprint sufficiently to produce corner lift.

    How Does the Two-Phase Morphology of High-Impact Polystyrene Translate into Print Performance?

    The two-phase polybutadiene-polystyrene structure controls impact and fracture behaviour. Under tensile loading, rubber-particle cavitation and craze formation increase energy absorption before failure; this is reflected in notched Charpy values for unfilled HIPS of approximately 10 kJ/m² when measured by ISO 179-1:2010 method 1eA. The rubber phase in HIPS typically has a particle size distribution between 0.5 µm and 4.0 µm; agglomeration during compounding can reduce impact performance and clog fine nozzles. In fused filament fabrication, the same rubber phase does not eliminate the inherent weakness at layer interfaces. The XY-plane tensile yield stress of the printed grey HIPS can be expected near the lower bound of the bulk extrusion-grade range, typically 20–30 MPa under ISO 527-2:2012 Type 1B, while Z-direction strength is strongly dependent on layer time, melt temperature, and chamber setpoint. Reported FFF anisotropy data for styrenics indicates that Z-strength may be 40–70% of XY-strength, which is a structural limitation rather than a product-specific defect. The flexural modulus of 1800–2200 MPa under ISO 178:2019 gives moderate stiffness; the material is less brittle than standard PLA but less rigid than fibre-filled grades.

    The grey grade differs from natural HIPS in optical density and surface inspection characteristics. Because the pigment reduces light transmission, the filament is not suitable for applications requiring translucency. The grey tone also allows surface scratches and layer lines to be evaluated under oblique white light without the glare of unpigmented styrenic material. This is relevant for visual inspection, not for mechanical performance.

    Table 1. Representative comparative data for unfilled FFF thermoplastics
    Property Test method Grey HIPS ABS PLA PETG
    Density ISO 1183-1:2019 1.04 g/cm³ 1.05 g/cm³ 1.24 g/cm³ 1.27 g/cm³
    Tensile yield stress ISO 527-2:2012 25 MPa 35 MPa 50 MPa 50 MPa
    Flexural modulus ISO 178:2019 2100 MPa 2000 MPa 3200 MPa 2100 MPa
    Heat deflection temperature Type B at 0.45 MPa ISO 75-2:2013 85 °C 95 °C 55 °C 70 °C
    Charpy notched impact method 1eA ISO 179-1:2010 10 kJ/m² 20 kJ/m² 3 kJ/m² 7 kJ/m²
    Melt volume-flow rate ISO 1133-1:2022 6 cm³/10 min at 200 °C/5 kg 5 cm³/10 min at 220 °C/10 kg 6 cm³/10 min at 210 °C/2.16 kg 8 cm³/10 min at 230 °C/2.16 kg
    Support removal medium — d-limonene insoluble insoluble insoluble

    The comparison shows that grey HIPS is not selected for maximum tensile strength or heat deflection; it is selected when impact-modified styrenic behaviour and solvent-removable support compatibility are specifically required. Unlike PLA, the material must be processed with a heated bed above 90 °C, which excludes many unenclosed FFF platforms. Unlike PETG, the HIPS surface can be solvent-welded with d-limonene or styrene-compatible adhesives, and unlike ABS it can be removed selectively from a model interface by the same chemistry. The grey pigment does not contribute measurable filler reinforcement; therefore the mechanical values remain within the expected range for unfilled high-impact polystyrene.

    Extrusion, Drying, and Machine Parameter Boundaries

    The filament is converted on single-screw compounding extruders with L/D ratios of 24:1 to 30:1, melt filtration at 40–60 µm, and vacuum venting. For FFF processing, a brass or hardened steel nozzle of 0.4 mm nominal bore can be used because the formulation is unfilled; nozzle wear is not expected to differ substantially from unfilled ABS. The measured melt temperature at the nozzle should be held between 230 °C and 250 °C. The measurement should be made with an immersion probe rather than the control thermistor alone; thermistor offset may be 5–10 °C. Operation below 220 °C produces incomplete layer fusion and sharp embrittlement at the interface; operation above 260 °C with residence times beyond 45 min accelerates decomposition of the polybutadiene phase and shifts the grey colour toward yellow-brown. The bed setpoint is 90–110 °C for first-layer adhesion on polyimide tape or polycarbonate sheet. A heated chamber or enclosure should maintain 60–80 °C, with the upper limit dictated by extruder cooling capacity and stepper thermal limits; below 50 °C, edge lift of a 200 mm rectangular raft can exceed 0.5 mm unless additional brim or draft shields are used.

    Moisture control before printing is a boundary condition rather than an optional step. If the spool has been exposed to 60% RH for more than 48 h, drying at 60 °C for 3–4 h in a desiccant dryer with a dew point of -40 °C is required. The target moisture content is below 0.05 wt%. Drying above 70 °C should be avoided because spool flanges and the filament winding can deform and create binding; drying below 50 °C is ineffective for removing surface-bound moisture within production intervals.

    Table 2. Starting FFF process parameters for grey HIPS
    Parameter 0.4 mm nozzle 0.8 mm nozzle
    Nozzle setpoint 230–250 °C 240–255 °C
    Bed setpoint 90–110 °C 90–110 °C
    Chamber setpoint 60–80 °C 60–80 °C
    Volumetric throughput 4–8 mm³/s 12–20 mm³/s
    Retraction distance, direct drive 0.8–1.2 mm 1.5–2.0 mm
    Retraction speed 25–40 mm/s 20–35 mm/s
    Part cooling fan 20–50% after layer 2 10–30% after layer 2

    When the grey HIPS filament is deployed as a solvent-removable support in a dual-extruder platform, the model material should be ABS or ASA. The bed-temperature compatibility condition is the limiting constraint: PLA and PETG require beds below 70 °C, while HIPS support layers collapse or delaminate if the bed is below 90 °C. The support interface is printed with a soluble zone and a dense support roof; gap spacing between the support roof and the model underside is typically 0.20–0.25 mm for a 0.4 mm nozzle, but this value must be tuned with the specific nozzle diameter and layer height. Removal is performed in a heated ultrasonic bath containing 95% d-limonene at 25–40 °C. Thick fins of 2.0 mm may require 4–8 h; published removal-rate data for this specific Clariant grey grade is limited, so the time should be determined on a sacrificial geometry before production parts are committed. Unlike PVA, HIPS support does not soften prematurely in humid air, but it requires aggressive terpene chemistry and cannot be washed in water. Nitrile gloves, local exhaust ventilation, and waste-disposal compliance with the solvent supplier’s documentation are mandatory because d-limonene can dissolve styrenic surfaces and can become a hazardous waste depending on regional classification.

    D-limonene should be considered incompatible with polycarbonate and with certain acrylate-based build surface coatings; the solvent bath should therefore be isolated from the build platform. Ultrasonic agitation above 40 °C is also avoided when the model material is ABS with wall thickness below 1.0 mm, because the combined thermal and acoustic energy can induce localised creep at the support-to-model interface.

    When the Melt Temperature Drops Below 225 °C

    Process records from production-scale FFF cells show that the transient melt-temperature drop during high-speed infill can be a greater source of mechanical anisotropy than the nominal setpoint. If the actual nozzle-exit temperature falls below 225 °C for more than 3 s, the surface of the preceding layer may remain below the critical welding threshold, producing a matte interface and reduced Z-strength. The effect is measurable with tensile specimens printed in the Z-axis and machined to ISO 527-2:2012 Type 1B geometry; the ultimate tensile stress is commonly lower by 20–40% when the chamber is held at 50 °C instead of 70 °C. For the grey grade, the melt-temperature boundary is linked to the rubber phase: polybutadiene-rich domains degrade at high temperature but provide ductility only if the matrix has been thoroughly fused at the interlayer boundary.

    The failure signature of this under-temperature condition is not catastrophic delamination on the first layer; it appears as micro-voids aligned along the raster direction and an unusual white stress-whitening pattern when the part is flexed. The white pattern is a diagnostic indicator of craze formation but not a positive material property; it indicates that energy is being absorbed at the phase interface instead of being transmitted through a fully consolidated layer. The operator should therefore increase the hot-end setpoint in 5 °C increments, reduce the fan output by 10%, or slow the infill to maintain the interlayer temperature above the glass-transition-dominated welding window.

    For incoming raw-material qualification, diameter and ovality are measured with a two-axis laser gauge at 10 mm intervals over the first 5 m of spool. Acceptance bands of 1.75 mm ± 0.05 mm and ovality ≤0.04 mm are common; out-of-round can cause extruder backpressure variation and visible banding on the part surface. Lot-to-lot MVR should be verified by ISO 1133-1:2022 at 200 °C under 5 kg; a shift of more than 15% relative to the supplier’s batch certificate indicates a change in feedstock grade or moisture and regrind content. Pigment dispersion is checked by extruding a 0.5 mm strand and inspecting against a standard grey scale; agglomerates larger than 75 µm can clog nozzles below 0.4 mm. Storage should be in sealed polyethylene bags with desiccant at 15–25 °C and below 50% RH. Under these conditions, the manufacturer’s recommended shelf life for styrenic filament is generally stated as 12 months, but the product should be dried before use regardless of the calendar age if the bag has been opened.

    The filament is not certified for food-contact use unless the specific lot is validated under FDA 21 CFR 177.1640 or an equivalent migration study; the grey pigment and rubber phase are not a substitute for such validation. Compliance with RoHS Directive 2011/65/EU Annex II heavy-metal limits and REACH SVHC restrictions applicable at the date of supply is expected, but downstream users should verify the supplier declaration for the exact lot and import jurisdiction.