Продукты

Clariant Polylactic Acid Black 3D Printer Filament

    • Название продукта: Clariant Polylactic Acid Black 3D Printer Filament
    • Сайт Factroy: Округ Юду, Ганьчжоу, Цзянси, Китай
    • Запрос цены: admin@ascent-chem.com
    • Производитель: Ascent Petrochem Holdings Co., Limited
    • Свяжитесь сейчас
    Спецификации
    Код ТН ВЭД 979829

    Как аккредитованный завод Clariant Polylactic Acid Black 3D Printer Filament, мы соблюдаем строгие протоколы качества - каждая партия подвергается строгим испытаниям для обеспечения последовательных стандартов эффективности и безопасности.

    Упаковка и хранение
    Упаковка
    Доставка
    Хранение
    Применение Clariant Polylactic Acid Black 3D Printer Filament

    In low-volume consumer electronics housing development, the Clariant polylactic acid black 3D printer filament is processed on fused filament fabrication machines equipped with a 0.4 mm brass nozzle, a heated borosilicate bed plate, and a part-cooling fan that is kept off for the first 3 layers to control edge curl. Spools that have been exposed to ambient relative humidity above 60% RH are dried in a desiccant dryer at 60 °C for 4 h; the dryer return air is monitored until the dew point drops below -40 °C. The black pigment package changes melt-flow behaviour compared with natural PLA, and the extrusion multiplier is started at 0.98, with final adjustment made by measuring a printed calibration cube. Nozzle temperature is held between 200 °C and 220 °C depending on print speed. Condensation on the filament surface must be avoided because hydrolysis reduces molecular weight and produces foaming at the nozzle. Tensile coupons printed for cosmetic housing prototypes are conditioned at 23 °C and 50% RH according to ISO 291 before testing per ISO 527-2. Snap-fit features, screw bosses and living-hinge prototypes produced from black PLA are not accepted for high-cycle use; the material fails in a brittle mode at lower elongation than unfilled ABS grades used in production parts.

    CheckpointTypical range / limitReference method or equipmentFailure mode when exceeded
    Drying temperature60 °C for 4 hDesiccant dryer, dew point -40 °CHydrolytic chain scission, foaming at nozzle, reduced interlayer fusion
    Nozzle melt temperature200 °C–220 °C0.4 mm brass nozzleSurface oxidation, stringing, pigment agglomeration above upper limit
    Build plate temperature55 °C–60 °CPEI sheet on heated borosilicate bedEdge lift below lower limit; elephant foot above upper limit
    HDT-B under 0.45 MPaSupplied datasheet value; commonly 50 °C–60 °C for unfilled PLAISO 75-2 method BTool and fixture softening in heated cells
    Conditioning atmosphere23 °C / 50% RH for 48 hISO 291Dimensional drift and tensile variability

    What Limits Sustained Clamp Force in Black PLA Assembly Jigs?

    Assembly jigs and inspection fixtures printed from black PLA are restricted by creep response under continuous load. The heat deflection temperature obtained under the 0.45 MPa flexural stress of ISO 75-2 method B is commonly between 50 °C and 60 °C for unfilled PLA, but HDT is a short-term thermal index and not a long-term allowable service stress. In a production cell where a fixture holds a workpiece under clamp force, sustained flexural stress is kept below the yield-stress fraction established from ISO 527-2 tensile data; otherwise locating surfaces develop viscoelastic indentation within 8 h to 24 h at 23 °C. The black pigment does not remove this limitation, and may increase surface heating under high-intensity inspection lighting, which accelerates creep in areas where the locating feature absorbs radiant energy. Fixtures for drilling, adhesive bonding and coordinate measuring-machine inspection are therefore printed with solid infill and thick ribs. The as-printed bores of drilling jigs are reamed after printing because thermal shrinkage produces undersized holes; the final bore size is verified after conditioning per ISO 291. Published long-term creep data for this specific Clariant grade under multi-cycle clamping are limited, so destructive testing on a printed beam per ISO 178 is required before fixture release.

    Investment casting pattern production uses black PLA as a sacrificial pattern material when the foundry can accept post-burnout carbon residue from the pigment package. The pattern is printed with solid wall structure and mounted to a wax tree before ceramic shell coating. Burnout is conducted in a forced-air kiln with staged temperature ramps: an initial hold below the melting range of the PLA, a second hold between 250 °C and 350 °C for volatilisation, and a final oxygen-rich soak at 850 °C to 950 °C to oxidise carbon-bearing residue. The black pigment system can increase the amount of carbon residue if the shell cavity is oxygen-starved; a post-burnout air purge is run until no visible smoke remains at the shell vents. Shell cracking from pattern expansion is reduced by designing a drainage cavity and using a burnout schedule that approximates wax removal. Published data for this specific configuration are limited; a shell trial on the actual pattern geometry is required to confirm clean burnout and ash content.

    Foundries using rapid shell cycles should not assume parity with natural PLA patterns because pigment decomposition products may alter the shell atmosphere. The pattern density can be checked by ISO 1183-1 to ensure consistent infill, and the burnout kiln is calibrated with a thermocouple at the pattern location to avoid local overheating of thin shell sections.

    Vacuum Forming Inserts and the HDT-B Limit

    Black PLA is used for vacuum forming inserts only when the forming sheet temperature remains below the continuous service limit of the grade. The ISO 75-2 method B value of unfilled PLA is commonly between 50 °C and 60 °C; high-impact polystyrene and PETG sheet are formed at 110 °C to 160 °C, which would soften an un-cooled PLA insert in the first pull. Low-temperature sheet operations using thin-gauge polyethylene or plasticised PVC can tolerate short cycles if conformal cooling channels and an aluminium backing plate extract heat between pulls. Vent holes of 0.6 mm to 1.0 mm are drilled through the insert after printing because layer-plane gaps create irregular airflow paths. The tool surface is sealed with a water-based epoxy to reduce water absorption and surface fibrillation. Undercuts are avoided because ejection forces can fracture layer lines. Tool-life data are not universal; each forming cell runs a 50-cycle trial with dimensional inspection of the formed part. If the surface temperature of the insert exceeds the HDT-B limit, the tool is returned to a lower sheet preheat or a metal-backed cooling circuit.

    For prototype tools, the as-printed insert is measured on a CMM before and after the trial to quantify creep distortion. The dimensions are compared with the CAD offset used on the tool, and the vacuum pump is isolated from the forming table to reduce vibration-induced crack growth. The use of black PLA in this context is restricted to prototype and short-run tooling; it does not replace filled epoxy or aluminium tooling in production cells.

    Technical training laboratories and metrology courses use black PLA for printed tensile bars and flexural specimens to demonstrate anisotropic mechanical response in additively manufactured parts. Specimens are printed to ISO 527-2 type 1A or ISO 178 dimensions, conditioned at 23 °C and 50% RH for 48 h, and measured with calibrated micrometers before testing. The black surface provides contrast against optical scanner backgrounds, which reduces edge detection errors in dimensional inspection exercises. Storage of the spools is in sealed bags with silica gel, and filament exposed below 40% RH is used directly without drying.

    When Black PLA Replaces ABS in Low-Temperature Snap-Fit Prototypes

    Substitution of black PLA into snap-fit designs originally specified for ABS requires re-analysis of assembly strain because the tensile elongation and fracture mode differ. The elongation-at-break value for the specific black PLA grade is taken from the supplier datasheet and compared with the ABS reference in the same ISO 527-2 conditioning state; the snap-arm deflection from an ABS part is not scaled directly. Cantilever hooks are thickened and the insertion face angle is increased to reduce outer-fibre strain during assembly. Because PLA is moisture-sensitive, the printed snap-fit parts are conditioned and assembled in a dry area; mould-release sprays are avoided if adhesive bonding follows assembly.

    Low-temperature service of black PLA snap-fit prototypes is restricted by the glass transition temperature of the grade. The Tg measured by ISO 11357-2 differential scanning calorimetry for PLA is typically around 55 °C to 60 °C; snap-fit retention force declines when the part is held above 40 °C. The material is not an acceptable ABS surrogate for under-hood, automotive interior or dishwasher-door trials, and evaluation is limited to ambient laboratory mock-ups. Where a true comparative test is required, the ABS and PLA beams are loaded in a universal testing machine under the same crosshead speed and thermal soak.

    Architectural Scale Models Require Enclosed Print Chambers.

    Architectural and topographical models printed with black PLA are produced on enclosed-frame machines because long wall sections and thin floor slabs warp when cooling air is applied unevenly. The build chamber is held at 30 °C to 35 °C, and the part-cooling fan is operated at reduced speed after the first 4 layers to reduce interlayer stress. A brim of 8 mm to 12 mm is added to floor slabs, and vertical walls above 120 mm are tied back to temporary supports. Dimensional stability is validated by printing a 100 mm × 100 mm flat tile and measuring bow with a feeler gauge under 0.5 N load. Z-axis tensile strength remains lower than XY strength because of interlayer fusion; destructive pull tests on printed coupons per ISO 527-2 are used to establish the orientation correction factor for stress analysis of the model.

    Large models are segmented along hidden panel joints to reduce cumulative shrinkage. The segment edges are machined flat and bonded with a solvent-free adhesive after conditioning at 23 °C / 50% RH. The black grade is not selected for models exposed to direct solar gain in glazed display cases unless the surface is protected from local heating above the HDT-B limit.

    Бесплатная цитата

    Конкурентные цены Clariant Polylactic Acid Black 3D Printer Filament, которые соответствуют вашему бюджету - гибкие условия и индивидуальные котировки для каждого заказа.

    Для получения образцов, цен или более подробной информации свяжитесь с нами по адресу +8618136850665 или отправить по почте admin@ascent-chem.com.

    Мы ответим вам как можно скорее.

    Телефон: +8618136850665

    Электронная почта: admin@ascent-chem.com

    Запрос

    Получите бесплатную сметуAscent Petrochem Holdings Co., Limited

    Гибкие условия оплаты, конкурентоспособные цены, первоклассное обслуживание — обращайтесь прямо сейчас!

    Сертификация и соответствие требованиям
    Более подробное введение

    Clariant Polylactic Acid Black 3D Printer Filament is supplied as a pigmented polylactide monofilament in nominal diameters of 1.75 mm and 2.85 mm. The commercial designation functions as the grade identifier; no separate numerical model code appears in the consulted technical literature. The compound comprises a semicrystalline PLA carrier resin and a dispersed carbon black pigment system at a loading below 2.0 wt%. Melt volume-flow rate, determined according to ISO 1133-1:2011 at 210 °C and 2.16 kg, falls in the expected range of 8 cm³/10 min to 14 cm³/10 min for this pigment-loaded class. Density is 1.24 g/cm³. Because published data for this specific black formulation is limited, property values in this document are presented as representative ranges for carbon-black-loaded PLA compounds with equivalent filler content rather than as batch-specific values for one production lot.

    Dimensional tolerance is specified as ±0.05 mm for 1.75 mm filament and ±0.07 mm for 2.85 mm filament, with ovality not exceeding 0.05 mm. The filament is commonly wound on 1 kg spools and sealed in aluminum-laminated packaging with desiccant sachets before shipment. Storage at 20 °C to 25 °C and 15% RH to 35% RH preserves the dried state; open-spool storage at 60% RH or higher requires pre-drying.

    What Distinguishes Black PLA from Natural and Impact-Modified PLA Filaments?

    The black grade differs from natural PLA mainly in optical density, crystallization behavior, and melt rheology. Carbon black acts as a heterogeneous nucleating agent; differential scanning calorimetry at 10 K/min typically shows an increase in peak crystallization temperature of 2 °C to 5 °C relative to unfilled PLA when dispersion median particle size remains below 5 μm. The nucleating effect can increase crystallinity after slow cooling and marginally raise the heat deflection temperature, but it can also reduce interlayer fusion at low nozzle temperatures because crystal growth competes with polymer chain diffusion. Compared with natural PLA, the black grade has lower translucency, higher melt density, and slightly lower melt strength. Compared with impact-modified PLA, the material has lower notched Izod impact strength and is not suitable for snap-fit components requiring ductile failure. The following table summarises representative comparative ranges for carbon-black-loaded PLA, unfilled PLA, and ABS.

    Representative comparative property ranges for carbon-black-loaded PLA, unfilled PLA, and ABS
    PropertyTest methodBlack PLA typical rangeUnfilled PLA typical rangeABS typical range
    Tensile strengthISO 527-2:201248–58 MPa50–65 MPa35–45 MPa
    Tensile modulusISO 527-2:20123.0–3.5 GPa3.1–3.8 GPa2.0–2.6 GPa
    Elongation at breakISO 527-2:20122.5–5.0%3.0–6.0%10–30%
    Notched Izod impactASTM D256-102.5–4.0 kJ/m²2.7–4.5 kJ/m²10–20 kJ/m²
    Heat deflection temperatureISO 75-2:2013 method B50–60 °C50–60 °C95–105 °C
    Melt volume-flow rateISO 1133-1:20118–14 cm³/10 min6–12 cm³/10 minNot directly comparable at the same condition

    Dispersion quality is a critical differentiator. If carbon black agglomerates exceed 20 μm, notched Izod impact strength can fall below 2.5 kJ/m² and elongation at break may drop to 1.5%. Masterbatch manufacturing on a 40:1 L/D twin-screw extruder with side feed at 60% of the barrel length is typical for achieving a median particle size below 5 μm. The pigment also raises melt density from approximately 1.08 g/cm³ to 1.12 g/cm³, which changes feed-zone compression behavior during filament extrusion. For applications requiring visible-light shielding, the black pigment provides high optical density and reduces translucency to less than 5% at 2.0 mm wall thickness. This is an advantage for light-shielding housings but a disadvantage for lithophane or backlit display parts.

    Pre-drying is mandatory at relative humidity above 60% RH or after open spool storage exceeding 8 h. PLA hydrolysis begins when moisture content exceeds 0.025 wt% at melt temperature; the visible failure modes are filament diameter instability, surface bubbles, and reduced tensile strength. Drying in a desiccant dryer at 60 °C for 4 h to a moisture content below 250 ppm is recommended, with a desiccant bed dew point of -40 °C or lower. Hydrolysis is autocatalytic and accelerates with carboxylic acid end-group concentration. At melt temperatures above 200 °C, moisture at 0.05 wt% can reduce molecular weight by 20% to 30% within 2 min, as measured by gel permeation chromatography. This is why closed-loop desiccant dryers are used instead of simple hot-air ovens in production. The black pigment can mask early yellowing, so moisture-induced damage may not be detected until tensile strength falls below 45 MPa. Incoming QC using a Karl Fischer titration method or a moisture analyzer calibrated for PLA should reject filament above 0.035 wt% moisture.

    On a production single-screw filament extrusion line with 25:1 L/D, 2.5:1 compression ratio, and melt pump, a typical melt temperature profile is 180 °C in the feed section, 210 °C in compression, and 205 °C at the die. The die diameter is 2.0 mm for 1.75 mm finished monofilament, and the draw ratio after air-gap cooling is 1.3:1. Batch-to-batch variation in carbon black dispersion can shift melt volume-flow rate by ±1.5 cm³/10 min; incoming QC should therefore include melt flow index testing and optical microscopy at 50× for agglomerate detection.

    When Melt Temperature Deviates Outside the Recommended Envelope

    The recommended nozzle temperature window for the black PLA filament is 190 °C to 220 °C. Below 185 °C, the melt viscosity rises sharply; carbon black raises low-shear viscosity more than high-shear viscosity, which can suppress oozing during travel moves but may cause under-extrusion and poor layer fusion. At 230 °C and above, PLA undergoes chain scission and lactide regeneration; the melt phase becomes increasingly Newtonian and strand melt strength collapses. Thermogravimetric analysis at 10 K/min in nitrogen indicates the onset of mass loss near 300 °C, but residence time above 230 °C for more than 5 min can already produce yellowing and molecular weight reduction. Capillary rheometry at 210 °C shows shear-thinning behavior; apparent viscosity at 100 s⁻¹ is typically 400 Pa·s to 800 Pa·s for PLA compounds of this melt flow class. The effective processing window is narrower than unfilled PLA by approximately 5 °C at the upper end when carbon black loading exceeds 1.0 wt%.

    Differential scanning calorimetry under 10 K/min nitrogen reveals a glass transition at 55 °C to 60 °C, cold-crystallization exotherm onset near 95 °C to 110 °C, and melting endotherm peak at 165 °C to 180 °C for PLA compounds of this class. Carbon black loading below 2.0 wt% raises peak crystallization temperature and reduces cold-crystallization enthalpy because the particles provide nucleation sites. Isothermal crystallization half-time at 110 °C is reported in the literature as 2 min to 5 min for unfilled PLA; carbon black can reduce this half-time by 10% to 30%. These kinetic parameters explain why heated chambers above 40 °C are not required and why bed temperatures above 60 °C can cause first-layer deformation under extrusion pressure.

    The upper print speed is limited by melt strength. At infill speeds above 80 mm/s with a 0.4 mm nozzle, the filament can exhibit melt fracture and irregular bead width because the apparent shear rate at the nozzle wall approaches the critical shear rate for PLA. A volumetric flow rate of 8 mm³/s to 10 mm³/s is stable; above 12 mm³/s, the melt transitions from plug-like flow to wall slip, and the extruder stepper motor may lose steps if the nozzle pressure drop exceeds 10 MPa. These values are observed on production FDM equipment for carbon-black-loaded PLA compounds and can vary with nozzle geometry.

    On a production FDM platform equipped with a direct-drive extruder and a 0.4 mm hardened steel nozzle, settings of 210 °C nozzle temperature, 50 °C bed temperature, 60 mm/s infill speed, and 0.8 mm retraction distance at 40 mm/s reduce stringing and maintain interlayer adhesion. Build plate adhesion is achieved on glass or polyetherimide beds with a polyvinyl alcohol-based adhesive at 50 °C; bed temperatures above 65 °C are not recommended because the contact surface approaches the heat deflection temperature. When printing a Type 1BA tensile specimen at 100% infill flat on the bed, interlayer tensile strength measured by ISO 527-2:2012 is typically 35 MPa to 45 MPa, or 70% to 80% of the bulk tensile strength. This reduction is attributable to incomplete polymer chain diffusion across the layer interface and is a known limitation of PLA FDM processing rather than a specific defect of the black grade.

    Regulatory Status and Material Safety Boundaries

    The compound is expected to conform to RoHS 2 2011/65/EU as amended by 2015/863 for lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, polybrominated diphenyl ethers, and the four restricted phthalates. REACH SVHC screening to 0.1 wt% per article is required for each batch because carbon black feedstocks may contain trace polycyclic aromatic hydrocarbons depending on the source and post-treatment. Carbon black as a bound pigment does not present an inhalation hazard during printing; however, sanding or machining printed parts can generate respirable particulate and should be performed with local exhaust ventilation. No claim is made for compliance with FDA 21 CFR food-contact provisions because black pigment systems and processing aids are not universally listed. The following checklist identifies the primary standards applicable to incoming inspection and printed-part qualification.

    Regulatory and standards checklist for Clariant Polylactic Acid Black 3D Printer Filament
    RequirementStandard or regulationApplicability
    Hazardous substance restrictionRoHS 2 2011/65/EU + 2015/863Electronic printing parts
    REACH SVHC screeningREACH 1907/2006/EC0.1 wt% threshold per article
    Tensile propertiesISO 527-2:2012Printed specimen quality control
    Melt volume-flow rateISO 1133-1:2011Incoming resin and filament
    Heat deflection temperatureISO 75-2:2013 method BThermal service limitation
    Notched Izod impactASTM D256-10Ductility screening

    Applications are limited to non-load-bearing housings, jigs, fixtures, signage, and visual prototypes that do not require continuous service above 55 °C. The black grade is not a replacement for ABS or PETG in under-hood automotive parts because the heat deflection temperature at 0.45 MPa is at least 35 °C lower. Against carbon-fiber-reinforced PLA, the black pigment grade has lower tensile modulus by roughly 1.2 GPa to 2.0 GPa and is non-abrasive to brass and hardened steel nozzles. Against PETG, the black PLA has lower impact strength and lower humidity resistance but higher stiffness and less stringing at equivalent retraction settings. Against ABS, the black PLA produces lower volatile organic compound emissions and lower shrinkage, but it cannot be acetone vapor-smoothed and has inferior thermal resistance. Chemical resistance is limited to weak acids and alcohols; esters, ketones, and strong alkalis cause stress cracking and should be avoided. The material is not intended for direct food-contact applications unless a specific regulatory grade is certified, because pigments and processing aids can migrate under aqueous and fatty simulants.